Model |
|
|
102GTN-PET |
||
|
|
|
|
|
|
|
|
||
|
|
|
AlOx Protective Coating |
|
|
Non-coated |
|||
|
|
|
|
|
|
|
|
||
|
|
|
Printability/lamination (AlOx side) |
|
laminated/ retortable |
||||
|
|
|
|
|
|
|
|
||
|
|
|
|
Hygienic standard |
|
|
conform to |
||
|
|
|
|
|
|
FDA |
|||
|
|
|
|
|
|
|
|||
|
|
|
|
|
|
|
|
||
|
Property |
|
Testing |
Units |
Typical values |
||||
|
|
|
|
method |
|
||||
|
|
|
|
|
|
|
|||
|
Thickness |
|
|
µm |
12 |
||||
|
|
|
|
|
|
|
|||
|
Density |
|
ASTM D792 |
g/cm3 |
1.38 |
||||
|
|
|
|
|
|
|
|||
|
Tensile Strength |
|
MD |
ASTM D882 |
MPa |
200 |
|||
|
|
|
|
||||||
|
|
TD |
210 |
||||||
|
|
|
|
|
|||||
|
|
|
|
|
|
|
|||
|
Elongation |
|
MD |
ASTM D882 |
% |
130 |
|||
|
|
|
|
||||||
|
|
TD |
110 |
||||||
|
|
|
|
|
|||||
|
|
|
|
|
|
|
|||
|
Haze |
ASTM D 1003 |
% |
1.51 |
|||||
|
Coefficient of Friction (uncoated side) |
ASTM D1894 |
/ |
0.48 |
|||||
|
Wetting Tension |
|
ASTM D2578 |
dyne/cm |
54 |
||||
|
(AlOx side) |
|
|||||||
|
|
|
|
|
|||||
|
|
|
|
|
|
||||
|
OTR |
|
ASTM D 3985 |
ml/㎡.24h |
1.34 |
||||
|
|
|
|
50%RH) |
|
||||
|
|
|
|
|
|
||||
|
WVTR |
|
ASTM F1249 |
g/㎡.24h |
1.08 |
||||
|
|
|
|
|
|
|
|||
NOTES:
1. Elongation of film should not exceed 2% during the production process, or the ALOx layer may crack then
2. Temperature should not be too high (generally below280℃) and the thickness should not excess 15μm
3. When using models without coated layer, the roll shaft which contact with the ALOx layer should be clean
4. The appropriate adhesive should be used when laminating, or may affect the peeling strength. Soft
5. The above information is for the customer’s reference only, and the actual situation should be verified